首页 > 标准下载>CNS 3564-4-2020 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验) 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验)\Rubber, vulcanized or thermoplastic - Determination of low-temperature properties - Part 4: Determination of low-temperature retraction (TR test)免费下载
CNS 3564-4-2020 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验) 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验)\Rubber, vulcanized or thermoplastic - Determination of low-temperature properties - Part 4: Determination of low-temperature retraction (TR test) CNS 3564-4-2020 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验) 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验)\Rubber, vulcanized or thermoplastic - Determination of low-temperature properties - Part 4: Determination of low-temperature retraction (TR test)

CNS 3564-4-2020 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验) 硫化或热塑性橡胶-低温性质之测定-第4部:低温回缩测定法(TR试验)\Rubber, vulcanized or thermoplastic - Determination of low-temperature properties - Part 4: Determination of low-temperature retraction (TR test)

  • 标准类别:
  • 标准大小:
  • 标准编号:CNS 3564-4-2020
  • 标准状态:现行
  • 更新时间:2023-09-06
  • 下载次数:
标准简介

本标准规定拉伸的硫化橡胶之温度-回缩特性测定法。 本标准并不包含所有热塑性橡胶,因许多热塑性弹性体在伸长率5 %~20 %范围具有降伏点,当热塑性橡胶进行TR试验时,此一事实可能影响结果,宜谨慎分析此等试验所得之结果。

标准截图
下一条:返回列表